The types of tests and investigations in the following allow for the assessment of the state of preservation and estimation of the strength and performance capacity of wood elements. The planning of the type and number of investigations is carried out following a thorough visual survey, which makes it possible to identify the most stressed areas, critical sections and the presence, location and extent of defects, as well as the geometry of the elements and the static patterns of the structure.
TESTS THROUGH PILODYN
Tests through Pilodyn make it possible to locally and globally assess the consistency of the woody matrix, allowing its density (average or characteristic) to be estimated through appropriate correlations.
The principle of operation is to drive a punch (cylindrical shape – diameter equal to 2.5 mm) into the woody matrix at constant energy (6 Joule = 6Nm), measuring its penetration depth in millimeters.
Based on the measured data, the density of the woody material is estimated through various correlations from literature, thus assisting in the identification of the woody species to which the elements under investigation belong.
RESISTOGRAPHIC TESTS
Resistographic tests make it possible to detect density variations within wooden elements, providing important indications of the characteristics of the wood and highlighting the presence of defects, anomalies and alterations, rotting, cavities, and knots.
The principle of operation is that of an instrumented drill capable of recording the resistance opposed by the wood to the entrance of a special drill bit, with a 3mm diameter end and thinner stem, equipped with a combined movement of rotation and advancement at a constant speed that can be preselected in relation to the density of the wood to be examined. This yields a measure of penetration resistance, a function of depth, that correlates with the density of the wood being investigated.
MOISTURE MEASUREMENTS
In the elements under investigation, tests are always supported by moisture measurements by means of a wood thermo-hygrometer.
An instrument specifically dedicated to measurements on wood is used for the purpose by virtue of the storage within it of correction curves and calibration of measurements based on the wood species. Specifically, calibration data are based on performing standardized tests on specimens whose moisture content is controlled in a kiln in the range from 7 percent to saturation. The instrument is calibrated for tests conducted at a temperature of 20°. Use of the instrument with the temperature probe allows immediate correction, performed in the background by the instrument itself, of the measured moisture value to obtain automatically temperature-corrected (ATC) moisture values.
Moisture measurements allow estimating the risk of biological attack on the investigated elements: as widely documented in the literature, the biological risk (fungal, insect or bacterial attacks) depends essentially on the moisture content of the wood.
VISIBLE CLASSIFICATION OF WOODEN ELEMENTS
Visible classification makes it possible to estimate the strength and stiffness of newly manufactured or existing wood elements by categorizing them into strength classes with reference to and in accordance with the respective industry standards.
This classification is based on the evaluation of defects on the inspectable faces; in particular, chamfers, size of knots (and groups of knots), inclination of the grain, presence of shrinkage cracks or various lesions are analyzed.
The classification can also be applied to in-situ wooden artifacts by means of in-situ inspections, which are often required in the field of cultural heritage. This classification system, which is in fact conditioned by the visual accessibility of all faces of the elements (lateral surfaces and heads) provides for the assignment of each structural element or each critical zone of the individual element (the concept of “critical zone” for in-situ elements) to a particular “in-place category,” to which correspond certain strength characteristics depending on the wood species.
VERIFICATION OF DELAMINATION OF GLUED WOOD ELEMENTS
“Delamination” is defined as a “separation of the layers of wood elements glued together due to either lack or loss of adhesion at the interface or loss of cohesion within the adhesive layer or one of the adhesives.” This loss of adhesion coincides with an absence of mechanical strength, which adversely affects the structural load-bearing capacity of the artifact. It is for this reason that the identification and quantification of delaminations is of paramount importance to estimate by how much the load-bearing capacity of the beams has been reduced.
Through the photogrammetric survey of the surfaces of glued wood elements and the sinking of special thickness gauges inside the respective glue joints, it is possible to identify the rate of delamination of the elements themselves. The reporting of said surveys is done by mapping the detected delamination depths.
ULTRASONIC SURVEYS
Ultrasonic surveys of wood involve the delivery of sound pulses by means of ultrasonic probes with frequencies between 20 and 70kHz. Based on the measured time-of-flight for said pulses and the measurement of the distance between probes, the apparent transmission velocity can be deduced, through the mapping of which the density of the wood matrix can be estimated and any internal anomalies identified.
DETECTION BY AUSCULTATION OF XYLOPHAGOUS INSECTS
The survey involves auscultation of the wooden element by means of a very high-sensitivity microphone station; it is then possible to detect the presence of ongoing attack by xylophagous insects, planning appropriate countermeasures.
ENDOSCOPIC INSPECTIONS
The investigation involves verification by direct vision of any internal deterioration in the wooden elements that may have been identified by other methods (resistographic survey, ultrasonic survey, …). The test consists of drilling in the wooden element a hole of maximum diameter and depth determined at the planning stage. Following thorough cleaning of the hole, the endoscopic probe is inserted, proceeding slowly, with inspection of the interior of the element under investigation, acquisition of photographic and video images to account for what was found. Tasq has high-resolution wireless endoscopes with an articulating probe to ensure the best possible endoscopic output.
VERIFICATION OF WOODEN STRUCTURES SUBJECTED TO FIRE
The investigation involves the evaluation of the depth of carbonisation as a result of fire, through the joint application of some of the previously described techniques. It is possible, depending on the Client’s requirements, to identify damage in well-defined sections of the burned element or to proceed with section-by-section verifications with a certain step along its axis.